Efflorescence on bricks is a white, powdery deposit of salts left behind when water moves through brick or mortar and dries at the surface. At Brick Cleaning Specialists Illawarra we see it most on new Illawarra homes in the first 3 to 12 months. It is usually harmless, but if it keeps coming back, water is still getting in.
If your new brickwork has turned white after the first heavy rain, you are not alone. Here is how to tell what you are looking at, what not to do, and when it is worth getting someone to look at the wall.
Prefer to listen? Hear this as a podcast episode on The Service Hub.
What causes efflorescence on new brickwork?
Bricks, blocks and mortar all hold soluble salts. When water moves through the wall, it dissolves those salts and carries them to the surface. The water evaporates and the salt stays behind as a white bloom.
New homes have a lot of construction water still inside the brick and mortar. As the wall dries out over the first few months, that water brings salts to the face as it goes. That is why so many new homes in estates like Calderwood, Tullimbar and Shell Cove show a white bloom after the first wet spell.
Is it efflorescence or lime staining?
This is the first thing to work out, because the two need very different treatment. Try a simple test on a dry day:
- Efflorescence is white, powdery and slightly fluffy. It brushes off dry and wipes to dust.
- Calcium or lime staining is white, hard and crusty, and sometimes looks glassy. A fingernail will not shift it.
Lime forms when lime from cement leaches out, reacts with the air and hardens into a crust bonded to the surface. It is harder to remove and needs acidic chemistry with proper dwell time. You can read more about it on our calcium and lime removal page.
Several masonry stains look alike and need opposite chemistry. Using acid on the wrong one can turn a removable stain into a permanent one, so if you are not sure, ask before anything goes on the wall.
Will efflorescence go away on its own?
Often, yes. The bloom on a new building is called primary efflorescence. It is normal, it is usually heaviest after the first wet spell, and it reduces a lot over the first year as the wall dries out.
Secondary efflorescence is different. It shows up later, or keeps coming back after the wall has been cleaned. That means water is still reaching the brickwork from somewhere. If it has been more than about twelve months, or it returns after cleaning, something is letting water in.
Where is the water coming from?
When efflorescence keeps returning, these are the usual suspects:
- a blocked weep hole
- a failed damp proof course
- roof or gutter overflow running down the wall
- a garden bed built up above the damp proof course
- irrigation spraying onto the brickwork
- a planter or balcony draining through the structure
Cleaning the wall without finding the source just resets the clock. When we clean efflorescence, we report what we can see, such as weep holes, ground levels, drainage and irrigation, so the cause can be dealt with by whoever needs to fix it.
What should you not do?
Most of the remediation work we do is fixing someone else's clean. With efflorescence, three things make it worse:
- Pressure washing it. Water dissolves the salt and drives it deeper into the brick, so it comes back.
- Sealing the wall while it is still blooming. The salt gets trapped behind the surface and can push the face of the brick off. This is called salt attack, and it is far more serious than the white bloom.
- Scrubbing a whole wall with vinegar. It might lighten a small patch, but on a wall it often leaves a patchy finish and its own salts behind, and it does nothing about the water.
How is efflorescence properly removed?
Order matters, and most failed attempts get it backwards. A lot of light efflorescence is loose crystal and comes off with a dry brush. Bonded deposits need a proper efflorescence remover or a correctly diluted mild acid on a saturated wall, then the wall is neutralised and rinsed well so no fresh salts are left behind.
Then comes the important part, finding the water. You can read the full process on our efflorescence removal page.
Does efflorescence damage brickwork?
The white bloom itself is cosmetic. What it can signal is not. Water moving through masonry year after year can wear down the mortar, attack the brick face with salt and eventually cause spalling, where the surface of the brick breaks away. Long running efflorescence is a warning worth acting on.
Frequently asked questions
How long after building does efflorescence appear?
It usually shows in the first 3 to 12 months after construction, and is often heaviest after the first wet spell as the wall dries out.
Can I brush efflorescence off myself?
Light, powdery efflorescence often comes off with a dry brush. Do not wet it first, because water dissolves the salt back into the brick.
Should I seal my bricks to stop efflorescence?
Not while it is still active. Fix the water first, let the wall dry and settle, clean it, and only then think about a breathable sealer.
How do I find out what the white stain is?
Send us two clear photos in daylight, one close up and one of the whole wall, and we will tell you what you are looking at. There is no charge to quote.
Get a straight answer on your white brickwork
We are Think Brick accredited, fully insured and based at Warilla, working across the Illawarra, the Shoalhaven, the Southern Highlands and the Sutherland Shire. Call or text photos to 0448 882 780, Monday to Saturday, 7am to 5pm.
Brick Cleaning Specialists Illawarra
Warilla NSW
Phone: 0448 882 780
Find us on Google Maps